| Diameter | 1,75 ± 0,2 mm |
| Printing temperatuer | 175-200 ℃ |
| Heated Bed Temperatuer | 50-80 ℃ |
| Tichtheid | 1,25 ± 0,05 g/cm3 |
| Heat Deflection Temperatuer | 50-60 ℃ |
| Melt Flow Rate | 5-7 g/min (190 ℃ 2,16 kg) |
| Treksterkte | ≥ 60 Mpa |
| Bending Strength | ≥ 70 Mpa |
| Ferlinging by Break | ≥3,0% |
| NW | 1,0 kg |
| GW | 1,3 kg |
| Lingte | ≈ 330 m |