| Diameter | 1,75 ± 0,2 mm |
| Printing temperatuer | 220-250 ℃ |
| Heated Bed Temperatuer | 70-100 ℃ |
| Tichtheid | 1,05 ± 0,02 g/cm3 |
| Heat Deflection Temperatuer | 70-80 ℃ |
| Melt Flow Rate | 2-4 g/min (190 ℃ 2,16 kg) |
| Treksterkte | ≥ 40 Mpa |
| Bending Strength | ≥ 60 Mpa |
| Ferlinging by Break | ≥ 10,0% |
| NW | 1,0 kg |
| GW | 1,3 kg |
| Lingte | ≈ 400 m |